水系钠离子电池钛酸亚磷酸盐阳极:进展和展望
|
|
王明理, 苏雪颖, 单政翔, 杨书哲, 郭恒瑞, 罗浩, 晁栋梁
|
The NTP Anode for Aqueous Sodium Ion Batteries: Recent Advances and Future Perspectives
|
|
Ming-Li Wang, Xue-Ying Su, Zheng-Xiang Shan, Shu-Zhe Yang, Heng-Rui Guo, Hao Luo, Dong-Liang Chao
|
|
| |
Fig. 4. Summary of construction of the advanced NTP anodes. (a) Ex-situ XRD pattern for Na2Ti3/2Mn1/2(PO4)3 at various charge/discharge states. Reproduced with permission of Ref. [45]. Copyright 2019, Royal Society of Chemistry. (b) Local structures of NTFP obtained by Rietveld refinements and (c) charge/discharge curves of NTFP/C tested in an aqueous half-cell at 2C rate. Reproduced with permission of Ref. [25]. Copyright 2019, Royal Society of Chemistry. (d) TEM image of the Na3MgTi(PO4)3. Reproduced with permission of Ref. [48]. Copyright 2017, Wiley-VCH. (e) TEM image (inset: magnified TEM) of the hollow NTP. Reproduced with permission of Ref. [18]. Copyright 2022, Wiley-VCH. (f) The microstructures of the NTP@C. Reproduced with permission of Ref. [49]. Copyright 2022, Wiley-VCH.
|
|
|
|
|