Research Progresses in Ni-Co-Mn/Al Ternary Concentration Gradient Cathode Materials for Li-Ion Batteries
Chun-fang ZHANG, Wen-gao ZHAO, Shi-yao ZHENG, Yi-xiao LI, Zheng-liang GONG, Zhong-ru ZHANG, Yong YANG
图7 (A, B) NCA82和(C, D) TSFCG85 电极充电到4.3 V后分别在55 °C下老化0和2天的横截面SEM图像. (E-G) NCA82和(H-J) TSFCG85正极材料分别充电到4.3 V后在55 °C下老化0、1和3天的横截面高倍SEM图像[55]. 经许可转载,版权所有2017 WILEY-VCH.
Fig. 7 Cross-sectional SEM images of (A, B) NCA82 and (C, D) TSFCG85 electrodes aged for 0 and 2 days at 55 °C after being charged to 4.3 V. High-magnification cross-sectional SEM images of the aged (E-G) NCA82 and (H-J) TSFCG85 cathodes aged for (H) 0, (I) 1, and (J) 3 days at 55 °C after being charged to 4.3 V[55]. Reprinted with permission , Copyright 2016 WILEY-VCH.